Skip to main content

[MW:3657] Re: Regarding PQR/WPS

Gents,

Normally 6010 preferable for root, high root penetration, cap and
filling can use 6013,

Mujib
Blng _ awe.
Brunei

On 11/15/09, AGUSTIN JIMENEZ <agumarca@yahoo.com> wrote:
> If you can do it
> , But I recommend using 6010 best in all passes, is preferable.
>
> Agustin Jimenez
>
>
>
>
> ________________________________
> De: Santhosh V S <santhosh.1974@yahoo.com>
> Para: materials-welding@googlegroups.com
> Enviado: sáb, noviembre 14, 2009 1:03:38 AM
> Asunto: [MW:3649] Re: Regarding PQR/WPS
>
>
> Dear All,
>
> I have one PQR for SMAW process and welding electrodes used for
> qualification are E6010 (root) and E6013 (for sebsequent passes). Anybody
> can advise me whether I can develop a WPS from this PQR with E6013 welding
> electrode for both root and other passes.
>
> Regards
>
> Santhosh
>
> --- On Fri, 11/13/09, Pablo Acelajado <pjacelajado@npc.com.sa> wrote:
>
>
>>From: Pablo Acelajado <pjacelajado@npc.com.sa>
>>Subject: [MW:3648] RE: 3639] Re: Criteria of HIC testing CSR, CTR and CLR
>> ratio.
>>To: materials-welding@googlegroups.com
>>Date: Friday, November 13, 2009, 3:46 PM
>>
>>
>>
>>November 13, 2009
>>
>>Please use NACE TM0284:2003. Thanks.
>>Pablo
>>SAVE TREES  - THINK BEFORE YOU PRINT
>>
> ________________________________
>
>>From:materials-welding@googlegroups.com [mailto:
>> materials-welding@googlegroups.com ] On Behalf Of Ramprasad Chari
>>Sent: Thursday, November 12, 2009 7:31 AM
>>To: materials-welding@googlegroups.com
>>Subject: [MW:3639] Re: Criteria of HIC testing CSR, CTR and CLR ratio.
>>
>>In my opinion,client needs to specify "crack resistance service" desired by
>> them.Like SOHIC & SZC are to be done for some severe conditions especially
>> applicable for Plates.HIC resistance is more critical and calls for a
>> controlled chemistry of elements especially Sulphur level.Severity is
>> decoded by partial pressure of H2S and its mole fraction.Again as per my
>> understanding "generalized" compliance to NACE std may not be correct.
>>If you refer page 41(Annexe E) of the std,it calls for confirmation by
>> Material Purchase i.e.Customer.
>>Hope I have made myself clear.
>>Regards
>>Aarpee
>>On Thu, Nov 12, 2009 at 8:23 AM, Bagesh Kumar <bagesh.kmr@gmail.com> wrote:
>>Dear All,
>>        I have gone through the Nace MR 0175/ISO 15156, the HIC and SCC has
>> to be carried out on the materials according to the standard.
>>Now I have gone through a project specification in which the client has
>> specified clearly the requirement of HIC Testing, SSC testing on Pipes,
>> Fittings, and Valves separately apart from the above stated standard
>> requirement.
>>Another Project specification of different client do not specify these
>> testing separately but they desire the materials to be according to NACE
>> MR 0175/15156,
>>My question remains: Is HIC and SSC testing mandatory on all piping
>> components for SOUR Services? if yes then please get me the code reference
>> for it.
>>And also illustrate the CSR (Crack sensitive ratio) other two results like
>> CLR and CSR.
>>The discussion on the chapter shall be appreciated.
>>Thanking You.
>>Bagesh.
>>
>>
>>
>>
>>
>>
>>>
>>
>
>
>
> ____________________________________________________________________________________
> ¡Todo sobre la Liga Mexicana de fútbol! Estadísticas, resultados,
> calendario, fotos y más:
> http://espanol.sports.yahoo.com/
> >
>

--
Sent from my mobile device

K.Mujibur Rahuman.
00673 7170703

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...