Monday, October 5, 2009

[MW:3453] Re: Welding consumables certification

Hi Sir,
 
I feel the diffrence is the following,
 
2.2 – this is a statement of compliance with the order, with indication of results of non specific inspection by manufacturer.

 

3.1 – this is a statement of compliance with the order, with indication of results of specific inspection by manufacturer's authorized inspection representative independent of the manufacturing department.
 
Kind regards
Raphy Joseph
 
On 10/5/09, ELAMARAN RAJAN <elams.rajan@gmail.com> wrote:
Dear Friends
 
As per our client specification for all welding consumables has to be minimum of EN10204 3.1 certification is required.
we are submitted EN10204 3.1 Chemical composition and for mechanical properties EN10204 2.2.
But Client not accepting that certificate due to mechanical properties has to be certified as per EN10204 3.1
 
let me know what is the difference between EN10204 3.1 and EN10204 2.2

regards
maran
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...