[MW:3428] RE: 3408] prequalified wps

No, not if conformance to AWS D1.1 is required.
 
Section 3, Prequalification of WPSs, paragraph 3.3, Base Metal / Filler Metal Combinations states, in part, "Only base metals and filler metals listed in Table 3.1 may be used in prequalified WPSs.  ( For the qualification of . . . base metals and filler metals not listed in Table 3.1 see 4.1.1.) 
 
There is no provision for "equivalence" of materials - either it is certified by the mill as one of the materials listed in Table 3.1 or it is not.  If not it must be qualified by test (PQR).
 
John


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ali Asghari
Sent: Saturday, October 03, 2009 7:31 AM
To: materials-welding@googlegroups.com
Subject: [MW:3408] prequalified wps

Hi FRIENDS
is it possible to write a prequalified wps for ST37 according AWSD1-1?(THIS MATERIAL NOT LISTED IN TABLE 3-1,BUT HAVE SIMILLAR COMPOSITION WITH SOME LISTED )
REGARDS.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...