Re: [MW:10647] Titanium to carbon steel welding

Dear Vijay,
1. No other way for pressure vessel. you may designed short saddle made by titanium then extended by C.S support. connection by bolting.
2. -

On Tue, Apr 12, 2011 at 7:39 AM, vijay <vijayakumarme@gmail.com> wrote:
Dear Friends,

There is a requirement mentioned in our client spec about Titanium to Carbon steel welding(Attached picture have more details).
I searched for literatures on this and I found that by normal fusion welding process is not recommended.
1. Is there any way,welding can be done between Titanium and carbon steel?
2. If YES or NO(on both case), please send a evidence document to confirm(like ASME,ASTM).
This is very urgent requirement.

Thanks in advance

Regards,
Vijay

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,

T. Rizal Hidayat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...