Mr.William,
 
No
 
Std. test positions have the following limits, 
  1. ± 15 from the horizontal plan
  2. ± 5  from the vertical planes
How will you make single test coupons which will cover the 3G & 4G position based on the above limits.
 
Pls understand the "QW461.1 Positions of welds-Groove welds" .
 
Regards,
 
K.Babu
Singapore
 
 
----- Original Message -----
Sent: Monday, August 23, 2010 4:27 PM
Subject: RE: **** SPAM **** Re: [MW:6650] weld test positions

 Mr Babu,

So if I qualify the welders on production weld I can then give them 3G & 4G qualifications is that what you are saying?.

Regards

Bill

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu
Sent: Monday, August 23, 2010 11:11 AM
To: materials-welding@googlegroups.com
Subject: **** SPAM **** Re: [MW:6648] weld test positions

 

William ,

 

80 degree is allowable tilt in the production weld not for the qualification purpose.

 

Regards,

 

K.Babu

Singapore

 

----- Original Message -----

From: William Lusk

Sent: Monday, August 23, 2010 3:24 PM

Subject: [MW:6643] weld test positions

 

Guys,

In accordance with ASME IX QW461 positions.

If I test welders on plate and tilt the joint to 80 degrees does that mean on one test butt weld I can qualify my welders for 3G and 4G?

Comments please.

 

Lusk

Senior Welding Engineer

Tel. : +966(4)3961171

Ext. : 344

Mobile+966 55 880 0431

E-mail : william.lusk@yanbusteel.com

billlusk66@yahoo.com

 

 


This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.



This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...