Wednesday, August 4, 2010

Re: [MW:6305] RE: 6250] clad welding

Yes, You are right. I have experienced that during back gouging people remove the CS and groove is extended up to cladding and during filling up CS groove, CS wire(weld metal dilute with the cald portion and cracks observed in RT.

Even in thicker section where double V is required back cladding would be similar to like welding from inside. For pressure vessels it is usual to have double V with wider caldding on inside (no choice).

On 3 August 2010 15:30, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
CKP
When you go for inside bevel? clad restoration area will be more in that case!


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chaitanya Purohit
Sent: Tuesday, August 03, 2010 4:50 PMSubject: Re: [MW:6285] RE: 6250] clad welding


see attached file for better clarity.

On 2 August 2010 17:21, Potter, Richard <RPotter@itses.com> wrote:
The base material 516-70 should be masked back so that the cladding is
about 1/2" back from the edge of the bevel on both sides.
You would then weld the 516-70 to 516-70 under your normal conditions.
After the required NDE is completed you would restore the 410 cladding.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of lusky
Sent: Monday, August 02, 2010 6:44 AM
To: Materials & Welding
Subject: [MW:6250] clad welding

I have to weld SA516 Gr 70 which has a 410 clad backing has anybody
done this? if so how were the results, there is no PWHT involved. 25mm
thick plate for a pressure vessle.
I have to qualify a PQR would be interested to read all comments





--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...