Re: [MW:32172] Most important to be verified or checked before starting weld Cladding Material

refer 02-SAMSS-012 & 01-SAMSS-044

On Tue, Apr 6, 2021 at 11:27 AM PK M <pkmqaqc@gmail.com> wrote:

Dear Experts,

What is the most important to be verified or checked before starting weld Cladding Material ?

Specifically for the clad materials- 625,825.

Any precautionary step to be taken before start the welding,

Any Special Advisable.

Thanks in Advance.

PKM.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_neLBzwYRyULxdDeZVkxbZ-8ctZH2x3cTgp97jZQ0zsz9Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANhkty4BmcYocKk2my-0N_py_m6x%2BV8WM3_x5abegeR-fBSqxw%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...