Re: [MW:32167] Any Special requirements for weld cladding or weld cladding materials ? ( Especially Saudi Aramco )

Refer SAES specifications  - SAES-W-100 will guide you for  cladding requirements 



On Tue, Apr 6, 2021 at 8:31 AM PK M <pkmqaqc@gmail.com> wrote:

Dear Experts,

Any Special requirements for weld cladding or weld cladding materials ? ( Especially Saudi Aramco ) 

Methods , Procedures and NDT requirements.

Thanks in advance.

PKM.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_ndbW_LPxCrdb5z0P-9sQBQAXU3u-2sK9aLqDiZU57xd4w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3N0iMaGV6Tmz%3DHXgvPF36jiRqLXt9fgKctY45QkYHjWng%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...