Re: [MW:32157] Difference between weld cladding, weld overlay and hard facing ?

Normally as per code there are 2 terminologies.

1. Corrosion resistance overlay which includes cladding.
       Cladding may be applied by below means
          a. Explosive cladding
          b. Hot roll cladding or bonding
          c. Weld overlay like Electroslag strip cladding, SAW strip cladding or any other welding process.

2. Hard facing overlay which is used for Wear resistance process


Thanks & Regards

J.Gerald Jayakumar




On Monday, 5 April, 2021, 12:20:49 pm IST, PK M <pkmqaqc@gmail.com> wrote:


Dear Experts,

Please explain the difference between weld cladding, weld overlay and hard facing ?

Thanks in advance.

Pkm.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_nfR6VrUrSzsog2tv%3DhnOcEj%2B4pPNxGmpW5RdGMANh1%3DbA%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...