10mm Carbon steel
No problem will be there.
Just carry out Visual Inspection of the weld and proceed for subsequent Welding
On Fri, 2 Apr 2021, 07:14 sankar bombay, <sankar.bombay@gmail.com> wrote:
cs materialOn Thu, Apr 1, 2021 at 11:59 AM Vishwas Keskar <vvkeskar123@gmail.com> wrote:what is the material being welded "CS ,Cr Mo or SS--On Thu, Apr 1, 2021 at 10:51 AM sankar krishnan <sankar.bombay@gmail.com> wrote:Dear All ,In our Pressure vessel project 10mm thickness plate they using (GTAW+SAW) process , They have welded GTAW with 4 mm of 10mm thickness and leave open for 1 days .. I like to Know what is the interruption limitations to stop welding Limits for <19mm thicknessPlease send me code documents--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ca6ac61-bff9-444e-bc40-80249c545c8dn%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OvQW%2BCv0cZt4DwxELXW15MwvN5R23UAQ52t4VV-Lcccw%40mail.gmail.com.
--shankar--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyDEeYRVztSMJz1fLmx_%2BfSGUR197JEKv5v78c7ND6iBqKrYw%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NxrpCLLH-VBWKhxwrXZmOxWKXO9YagYb3sqioZcvugkg%40mail.gmail.com.
Comments