Re: [MW:31685] Query related to F Number in welding

Ref ASME Sec9 QW- 433. 

On Mon, Nov 2, 2020, 2:30 PM NIKHIL THOMAS JOY <nikhil.thomasjoy@gmail.com> wrote:

Dear experts,

Greetings of the day

I have a query related to the F Number in welding process.

IF I QUALIFY A WELDER WITH F No.6, He can weld all F.No-6.

But, if I Qualify with F No.5, can he weld F No.1 to 4.

Experts please reply as per code reference.

BEST REGARDS,
NIKHIL THOMAS JOY
IWI LIMITED 
ADNOC-WHRP
0544975526

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJxkuiVye%3DvWpXy28w6g%2Bvj77vUNNQHJGZp6dUUi%2Bb5aD1oyOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM7A61wU_wvOFqoy%3DXyn9C0GXcin1vWTHL_mUw_BXox1g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...