David thank you for your reply. Can you tell me the reasoning behind slower weld speed.
On Thursday, April 9, 2020 at 5:31:09 AM UTC-5, d...@btinternet.com wrote:
-- On Thursday, April 9, 2020 at 5:31:09 AM UTC-5, d...@btinternet.com wrote:
Try a slower welding speed and a closer arc length.
Regards, 9 4 2020.
David Harvey
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ef1ee33e-99ba-43ce-a8c2-978055638d57%40googlegroups.com.