Dear Mr.Ali,

Refer attached welding consumable catalogue. It will  give some reference for welding of X22CrMoV12-1.

Navnitkumar Parikh

On Sat, 25 Apr 2020 at 11:31 AM, Waris Ali <waris.pk566@gmail.com> wrote:
Dear Experts 

X22 CRMOV12-1 +QT2 what is the requirements of mentioned welding and consumable please advised.


Waris Ali 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC23Ko3OAgNEhgd3CYR7A3EKw4aND_T-de5oBNcp7bf7L-exDA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKHZGHovt0RBrQhCrQOA9zJqRkR9aCU5EDiww2GfbXO0jhe7Gw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...