Please check attached Article for Pickling of Nickel alloys

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, April 15, 2020, 06:23:14 PM GMT+7, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


I suppose there are 2 types of Nickel Alloys, Solid solution strengthened and Precipitation Hardened alloys.

Inconel 601 falls under Solid solution strengthened and supplied in  Solution Annealed Heat Treated condition.

ASTM A 380 is pickling and passivation standard for stainless steel.

it is better to contact the Manufacturer regarding Pickling and passivation to remove corrosion deposits.

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, April 15, 2020, 05:57:26 PM GMT+7, harenath jha <harenathjha@gmail.com> wrote:


Again... Please what is the as shipped condition... If it is not heat treated then u can not do passivation. If it is heat treated then passivation can be done Please refer astm a 380 for more details...  Still you are in doubt please let me know..

On Wed, Apr 15, 2020, 12:56 Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear Harenath,

       Due to improper storage, the thermowell of Inconel 601 got corroded. For these items can we do pickling and passivation? 

On Wed, Apr 15, 2020 at 7:28 AM harenath jha <harenathjha@gmail.com> wrote:
What is the conditions of material.
Is it heat treated normalised or something else.

On Wed, Apr 15, 2020, 10:31 Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear all,

  Can any one suggest the specification or standard procedure s to be followed for pickling and passivation of inconel pipes and flange surfaces

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0xJKPZj%2Bf35s8imSXNUXKDy%3DEKgyqDtZadtu62dHMgHmw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOdz0Z-ti2%3DSPn1p1wh9g_1XHWJnG_TH%2B4OJbOMMg1Zkg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zGzo1KpqwbYDZ_NdHVkSfM3W2JNgb%2BSwVwnnhffkFC7w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOu7%2B2meFq%2B6P1crG%3DtW%2BpQ4oqK5czvqwUmqSp0PdG0QA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1079142675.549488.1586949209105%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...