Re: [MW:30755] Run-Out Length for SMAW Process

I think 350/450mm is the length of welding rod not necessarily the length of deposited length which can vary as per the thickness of layer deposited.

Regards

Chris

On Tue, Apr 14, 2020 at 08:08 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
I am not sure with the below mails but I can give explanation to Run-out Length.

In SMAW process, the distance welded by a single electrode (350/450mm length) and it is related to welding speed

Thanks & Regards

J.Gerald Jayakumar




On Monday, April 13, 2020, 07:17:45 PM GMT+7, Vishwas Keskar Welding Manager Pune India <vvkeskar123@gmail.com> wrote:


PL. EXPLAIN MORE 

What is this ?

> 100 mm is min 150 mm
< 100 mm is min 100 mm

Or you can apply simple logic:

Thickness of base metal / each layer height = No of layers * 10-20  mm (staggering length at each layer depending upon the process)



On Sunday, April 10, 2016 at 8:25:07 PM UTC+4, Maulik H. Thakkar wrote:

Dear sir,

Recommended run in run out length for base metal thickness;
> 100 mm is min 150 mm
< 100 mm is min 100 mm

Or you can apply simple logic:

Thickness of base metal / each layer height = No of layers * 10-20  mm (staggering length at each layer depending upon the process)

Regards,
Maulik

On Apr 10, 2016 2:25 PM, "Kurniatullah Sirajudin" <kurniatull...@gmail. com> wrote:
Dear Expert,

A week ago, i received comment regarding welding for smaw process.

My client ask to me, run-out length for smaw process.

I don't know what is run-out length.


Please advise me 


Thank you & Regards

Kurniatullah Sirajudin

--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@ googlegroups.com.
To post to this group, send email to material...@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ bb9ef69c-8c36-42e8-b090- 7dd6d32d8af3%40googlegroups. com.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e21dba0d-3601-4908-a012-deccee00c495%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1864291333.3272837.1586791670646%40mail.yahoo.com.
--
THANKS AND REGARDS
CHRIS SABU
0559695451

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACY3QXS9%3DoSHmeP8eftPk3Y%2BucNfU6mpNMbpFvW6My%2BkT9ee5g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...