The API 5L pipeline is commonly used for crude oil application.
ASTM-A-106B is very close to that .
X indicates minimum yield strength .
API 5L X65 pipe is a high level grade pipe in API 5L with minimum yield strength required in 65000 Ksi or 450 Mpa.
You can replace but take a view of your designer .
Regards
On Sat, 11 Apr 2020 at 12:41, Rouji <a.m.alrouji@gmail.com> wrote:
Greetings,--We have welded X60 crude oil pipeline, and we want to replace a small portion of the pipeline, can we use X65 as replacement?.Because we have stock of X65.Thanks.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eadfb524-1fc1-4f05-adae-de22c88a9b74%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OhVHCQ-8FFmM_vwi2qXAPvp3KXj5K7Ga18PPSaV%3DT1SFg%40mail.gmail.com.
Comments