[MW:30792] Heat input and cooling

Dear all
I am confused about the following statement. Can anyone tell me the reason.

High heat input causes slow cooling and low heat input causes fast cooling.

I understand that cooling is a function of temperature differences between the metal and ambulance system. If high heat input causes high temperature then temperature differential should be higher than low heat input.
Can any one tell me the reason.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/16692389-12f7-4b45-8ad4-e03a92e6c9b2%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...