Monday, January 7, 2019

Re: Re: [MW:28867] Re: Hot tap wps

Greetings,

Check 11.2.1 / 11.2.3 of 577 API RP and below link has very deep understanding to address the consequences / concerns of B.2.3.1.2 of 1104s API criticality in which and why it has been inlined to be mandated as essential.


(PDF) Temperature Prediction in Hot Tapping Process for High Pressure Pipeline. Available from: https://www.researchgate.net/publication/316961627_Temperature_Prediction_in_Hot_Tapping_Process_for_High_Pressure_Pipeline [accessed Jan 07 2019].


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
Date: 2019-01-06 08:35
Subject: Re: [MW:28866] Re: Hot tap wps
Hi All,

You can check API RP 2201 for Hot Tapping procedure.

Best regards,

Md Saidur Rahman, MASc
Deputy Manager (Operation)
Ashuganj Compressor Station
Gas Transmission Co. Ltd. (GTCL)
Contact: 01710553319; mdsaidur.rahman@ryerson.ca


On Sat, Jan 5, 2019 at 4:11 PM SARAVANAN KRISHNAN <saravweldingengineer@gmail.com> wrote:
Hi Puneet.

1. You can get the flow rate from the operation. (approximately) then will do the pqr with flow condition.or  if pqr already has done, follow the below steps. 
2. Based on the flow rate u can adjust the heat input value in the WPS( within the range).
3. while doing the hot tape parallel check the flow rate, current-voltage values,interpass temperature.

-- 
K. SARAVANAN. ME (WELDING TECHNOLOGY)
     WELDING ENGINEER,
     DOHA, QATAR.
     MOBILE: +974-77466433. 

On Tue, Jan 1, 2019 at 1:14 PM Mohd Siraj <mohd52100@gmail.com> wrote:
it is a flow rate that you mentioned in WPS.

qualified PQR with severe condition where cooling rate is high and chances of burn through is high.
that's meaning.

On Thursday, October 18, 2018 at 2:51:21 PM UTC+3, puneeta...@gmail.com wrote:
Dear Experts,

We are actually in the process of making WPS for Hot Tapping . in this context while referring to API 1104 , unable to interpret the below paragraph from API 1104 In Service welding .

Kindly help in understanding

B.2.3.1.2 Pipeline Operating Conditions


For in-service welds, an increase in the severity of the pipeline operating conditions (in terms of weld cooling rates)
above the group qualified constitutes an essential variable.

Thanks in advance

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...