Dear Kannayeram,

Yes I have checked in WPS and PQR in both A No- Is 1(Same).

Thanks and Regards
Kiran

On Wed, Jan 2, 2019 at 4:21 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
When ER 70S6 is in GTAW, have u checked A no ?
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Jan 2, 2019 at 7:49 AM muneebslsa@gmail.com <muneebslsa@gmail.com> wrote:
Hi,

Firstly you should check with your project approved line class / NDE matrix and PMS to know all the requirements, i suggest you to check with competant aramco approved welding engineer, but still find the clarity from my side and revert back if anything.

 a) What is the Base metal thickness Range and  Deposited weld metal range as per B31.3 for GTAW & B31.4 for SMAW.
REPLY
You shall check the welding code not construction code, for ASME IX check QW-451.

 b) As Per ARAMCO & Sec IX- AWS No(Class) ER 70S-2 / 3 can we use in WPS . but in PQR they have used only ER70S-6

REPLY
Yes agree with trailing mail ER70S-6 may increase hardness that is why there has been a  restriction in SA project for sour service, check latest SAES-W-011 and SAIC W 2031 of A8 or A9, still ER 70S-2 or 70S-3 may incorporate if you have already got your 70S-6 PQR / WPS approval with CSD, if not then it may restrict, i beleive CSD will not approve ER-70s-6 filler for sour service.

1) For Sour Service what are the test we required and what is the minimum and  maximum thickness qualification for WPS.

REPLY

Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
Date: 2019-01-01 18:55
Subject: Re: [MW:28844] Re: As per B31.3 2012 & Section IX
Why u have chosen ER70S6 for GTAW which is having high Mn,Si, which may increase the hardness. 

On Tue, 1 Jan 2019 5:48 pm Kiran <karan.hbl@gmail.com wrote:
Dear Siraj,

I have not understand your answer,

Please refer below tables i have mentioned PQR Ranges and also i mentioned My WPS Ranges.
Please check WPS table what i have given range is correct or not, and if not correct please tell me as per code.

        

PQR

 

 

 

 

 

 

 

 

Base Metals :

SA 105 to API 5L

 

 

 

 

 

 

 

P No :

1

Group No:1&2

 

To

P No :

1

Group No:1&2

 

Thickness :

25.4mm

 

 

 

 

 

 

 

Filler Metals:

ER70S-6

GTAW

&E 7018

SMAW

 

 

 

 

 

 

                                                               




WPS for Sour

 

 

 

 

Welding Process :  GTAW+SMAW

 

 

 

 

 

CODE:

IX

ASME : B31.3,B31.4 &SAES- W-011/012

 

 

 

 

 

 

 

 

 

 

 

 

QW-403

 

 

 

 

 

 

 

 

P No :

1

Group No:1&2

To

P No :

1

Group No:1&2

 

 

 

 

 

 

 

 

 

Base metal Thickness Range :(B31.3)

 

 

 

Groove: 5mm to ≤20mm

 

 

 

 

Base metal Thickness Range :(B31.4)

 

 

 

Groove: 5mm to ≤ 38mm

 

 

 

 

 

 

 

 

 

 

 

 

 

Deposit Weld metal  :(B31.3)

 

 

GTAW: Max 6mm,SMAW: Max 14MM

 

 

 

 

 

Deposit Weld metal  :(B31.4)

 

 

GTAW: Max 6mm,SMAW: Max 32MM

 

 

 

 

 

Maximum Pass Thickness:

 

 

≤13mm

 

 

 

 

 

 

 

 

 

 

 

 

 

 

QW-404

 

 

 

 

 

 

 

 

 

GTAW

 

SMAW

 

 

 

 

 

SFA No -

5.18

 

5.1

 

 

<p class="MsoNormal" style="margin-bottom:0in;margin-bottom:.0001pt;line-height: normal

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--

KIRAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...