Hi Puneet.
1. You can get the flow rate from the operation. (approximately) then will do the pqr with flow condition.or if pqr already has done, follow the below steps.
2. Based on the flow rate u can adjust the heat input value in the WPS( within the range).
3. while doing the hot tape parallel check the flow rate, current-voltage values,interpass temperature.
--
K. SARAVANAN. ME (WELDING TECHNOLOGY)
WELDING ENGINEER,
DOHA, QATAR.
MOBILE: +974-77466433.
On Tue, Jan 1, 2019 at 1:14 PM Mohd Siraj <mohd52100@gmail.com> wrote:
it is a flow rate that you mentioned in WPS.--qualified PQR with severe condition where cooling rate is high and chances of burn through is high.that's meaning.
On Thursday, October 18, 2018 at 2:51:21 PM UTC+3, puneeta...@gmail.com wrote:Dear Experts,
We are actually in the process of making WPS for Hot Tapping . in this context while referring to API 1104 , unable to interpret the below paragraph from API 1104 In Service welding .
Kindly help in understanding
B.2.3.1.2 Pipeline Operating Conditions
For in-service welds, an increase in the severity of the pipeline operating conditions (in terms of weld cooling rates)
above the group qualified constitutes an essential variable.
Thanks in advance
Regards,
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment