Tuesday, January 1, 2019

[MW:28836] Re: Calculation for root gap according to tihckness of pipe

Root gap is  not depend on pipe size or thickness,indeed it is based on process to be used for welding.
GTAW-4-5mm
SAMW-3.5-4.5mm
SAW-1.5-2.5mm

On Friday, July 22, 2011 at 2:17:46 PM UTC+3, abhishek ojha wrote:

Dear Expert,

Kindly guide me how to calculate root gap according tihckness of pipe of different /same dia.(different tickness but same dia)


Thanks & Regards,

 

Abhishek Ojha


 Engineer- Construction 


cid:image001.gif@01CA0B94.B49995B0

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...