Saturday, November 3, 2018

Re: [MW:28561] weld metal deposition calculation

Thank you Karthik for sharing this link.

Md Saidur Rahman, MASc
Deputy Manager (Operation)
Ashuganj Compressor Station
Gas Transmission Co. Ltd. (GTCL)
Contact: 01710553319; mdsaidur.rahman@ryerson.ca


On Sat, Nov 3, 2018 at 1:50 PM 'Karthik' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi,

the following link is better for u.


Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com



On Saturday, November 3, 2018, 12:48:02 PM GMT+7, Mithlesh <mithleshmech47@gmail.com> wrote:


Dear all

in attached file from where below yellow highlighted value taken not clear to me, help to clear.

=IF(D$6=1,(PI()*(C20-(2*D20)+(2*G20))*L20*0.1*0.01*7.85*0.001/(S$16*S$17)),0)

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...