Re: [MW:28561] weld metal deposition calculation

Hi 

But I can't implement this in excel for because over 19 mm edge preparation change and another thing is i am putting all the thing with root run to fill and capping with different different consumables size to calculate time for weld the joint. If you tell me about my query then it will better to me.

On Sat, 3 Nov 2018 at 1:20 PM, 'Karthik' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi,

the following link is better for u.


Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com



On Saturday, November 3, 2018, 12:48:02 PM GMT+7, Mithlesh <mithleshmech47@gmail.com> wrote:


Dear all

in attached file from where below yellow highlighted value taken not clear to me, help to clear.

=IF(D$6=1,(PI()*(C20-(2*D20)+(2*G20))*L20*0.1*0.01*7.85*0.001/(S$16*S$17)),0)

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
Sent from iphone

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...