[MW:28567] E 48XX welding consumable details

Kindly elaborate details of E 48XX welding electrode for SMAW welding.

Which welding rod to be used for the same category for structural steel welding with low cost & good quality of welding with strength.

you can share details of near around E 48XX series as well...

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...