Re: [MW:27762] AWS D 1.1 interpretation on Increase in Preheat / Interpass temperature

it is not like ASME sec9 and ISO 15614-1. your client comments is ok.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Wed, May 2, 2018 at 9:24 AM, N VENKATESWARA PRASAD <weldengr.velosi@gmail.com> wrote:
Dear Experts,

We have received a comment on Increase in Preheat temperature greater than 56°C is essential variable as per AWS D.1 from our client.

My interpretation is the increase in 56°C is applicable only for inter pass temperature.  The details are as given below. 

 

PQR   Test coupon thickness        :  30 mm

PQR   Preheat temperature          :  30°C

PQR Inter pass temperature        :  173°C

 

Job Thickness                                  : > 38 mm  to 65 mm  ( As per Table 3.3)

Preheat temperature                    :  110°C

Inter pass temperature                 :  220°C

MDMT                                               :  -40 °C

 

As per AWS D 1.1  Table 4.6  Point no. 7   an increase more than 56°C in max preheat or interpass temperature is essential variable  for CVN testing applications.

 

Based on the above clause, the client is insisting that the Qualified Range for  thickness in WPS shall be restricted to 38 mm as the preheat is increased from 30°C to 110°C which is not acceptable .

 

Please provide me if you any interpretation on it from AWS.

Regards

Prasad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...