Thursday, October 6, 2016

Re: [MW:25492] Cellulose electrode redrying

Dear all,
Please see and follow the recommendation from the manufacturer.
Please refer the packet of E6013, you can see that 15odeg C heating is recommended.

Regards,

Hareesh K V
+91-8547859202


On 6 Oct 2016 8:58 p.m., "Roy Joseph" <royjoseph04@gmail.com> wrote:
Cellulosic electrodes works better with 2-5% moisture in it.So re drying is not advised.

Regards,

Roy Joseph,
Oman

On Mon, Oct 3, 2016 at 10:13 AM, Pravin G <htcispravin@gmail.com> wrote:
Dear expert,

Can anyone advice why cellulose electrode don't need redrying? Any particular Technica reason?

Pravin Poornachandran

Sent from my iPhone

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/672D2E56-43BC-4AE9-8B4B-ED48562CB124%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAw5q51hTHsJ8Fy9smFk-NOSDm3-XCFeTMm%2BCVSvsD8igwC1%3DA%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAVtyV0e1dfRJr5hZX2E1LsrY-5-3M_2ze8SdRLZGU_S1g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...