Re: [MW:25492] Usage of ASME Sec 9 WPS for sub contractor

If the subcontractor is approved by the client (The agency which awarded the contract to you) then you can use subcontractor WPS.

The main  contractor WPS can be used by subcontractor as the work is awarded to the main contractor and it is only based on the internal work award system the main contractor have awarded the work to subcontractor and the welding control acticities are with the main contractor only.

Regards,

Hareesh K.V
+91-8547859202

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAXq3mjm2YAAD8juSSREE5hRRrt%3D3UGA9PF%3Du5oZTeT78w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...