Re: [MW:24409] Welding by SAW process is it mandatory for heavy thick vessels in H2 service

You may use SMAW with approved WPS and with expert welder but, as compared to SAW the productivity is too less, chances of defects are more, more workmanship required, more precise testing is required and no client will take chance for the delay and the quality. 

Regards,

Anosh Wankhade




From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Sent: Mon, 29 Feb 2016 11:10:12
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:24404] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
SMAW is a time consuming and quality purely based on welder skill. SAW process is also available in Semi-Automatic process, it is gives better quality of weld, fast, aesthetic look

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Sat, Feb 27, 2016 at 9:12 PM, <dilintas@gmail.com> wrote:
Almost 20 years ago I was in a tank farm project were field welds were performed by means of saw

Sent from my BlackBerry 10 smartphone.
From: Prasad
Sent: Σάββατο, 27 Φεβρουαρίου 2016 - 09:02
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:24384] Welding by SAW process is it mandatory for heavy thick vessels in H2 service

Dear welding experts,

We are manufacturing heavy wall vessels for H2 service.
MOC SA 516 Gr 70. Thick 56 mm
Due to large size vessels are to be supplied in two sections.
Hence on site weld joint will have to be done at place of installation.
At shop we are using SAW process for welding.
At field rotating is not possible and we want to use SMAW process.
Our client is asking us to use SAW process for field weld joint also.

We know that SAW is semi automatic & more productive process.

My question is whether is their any restriction to use SMAW process.

Request experts to give their valuable views to convience client technically.

Best regards,

Prasad Ghanekar


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb19d5b1-6c54-45fe-8e91-1346dd8c9617%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160227154234.6713426.85120.1966%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMGZGYtAK5gG1pnsB4W2OZ9KngLfpg5Mn4_MM1Nib1tGQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1456724412.S.18199.30999.f6-235-206.1456734926.27074%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...