I suppose you mean "verify" when you write "rectify". Unless you use huge magnets the max detection depth with MPI is no more than 2 mm

Sent from my BlackBerry 10 smartphone.
From: Mohammed Ghani
Sent: Δευτέρα, 29 Φεβρουαρίου 2016 - 05:19
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: RE: [MW:24403] Fillet weld cracks below 6 mm with suitable NDT.

Dear,

Thanks for the reply.

This is for RIG spudcan crack found after 3 years in service. .. I need to rectify if any more possible cracks available in fillet joints... usually with MPI we could locate cracks upto 5 to 6 mm...

Please prove me more suggestions.

Regards,
Mohammed ghani.

On 28 Feb 2016 17:18, "'Agustin Jimenez' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Hello

I recomend Phased Array ultrasonic technic.

Agustín
Level 2 VT PT MT UT RT


Enviado desde mi smartphone Samsung Galaxy.


-------- Mensaje original --------
De: Mohammed Ghani <ghani386@gmail.com>
Fecha:28/02/2016 04:31 AM (GMT-04:30)
Para: materials-welding@googlegroups.com
Cc:
Asunto: [MW:24396] Fillet weld cracks below 6 mm with suitable NDT.

Dear experts,

I want to locate Fillet weld cracks below 6 mm for 22 mm plate with double V  preparation.
Is there any special techniques from NDT I can use to identify cracks below 6 mm.

Please suggest me if any suitable NDT procedure for this. It is a bit urgent. 

Appreciate your respond.

Regards,
Mohammed ghani.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhBp4jWOun%3DrCPmJuh%2B1PLib%3D9%2BFM4KWDSsuRAUVRSVsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/h8u94emwh70urwdu19wnl0ig.1456666226993%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVhUaR90G2HdKQb8uuSxE5Ne_WhFkS0RksZdiMUwZ%2BWojw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...