Re: [MW:24356] How much welding to be finished

Carbon steel is not a problem, but alloy steel or high strength steel, minimum 6mm or 1/3 of thick before stopping welding

On 22-Feb-2016 4:20 pm, "pradip kumar Sil" <pradipsil@gmail.com> wrote:
Dear All,
Welding can be stopped ( Carbon Steel Material )How much percentage of welding finished.
I remember 33% to be completed at a time with non removal of slag.
Can anybody guide me to provide code reference.
Regards,
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3Dgp93tNBfryb%3D3Ar56eM60i%3DB0wk3mxm_z5KbZBiRy%3Dw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMShQDwqSG82xrs60w2ZfaeiEydvr%2Bo42wy%3D_TKwaxqQw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...