RE: [MW:24352] RE: 24334] Failure Analysis

Seems to me that it was tested above the minimum specified yield strength of the base material (over pressured) because there is a lot of deformation visible on the picture, if material/weld failures were present in general you will get a brittle fracture. Radiographic examination makes only sense if the present fracture surface shows any indication which may relate to an improper longitudinal weld.

I would suggest checking base material certificate (also check wall thickness with requirements) and execute some tests on the uninfluenced base material in order to check if values comply with the certificate.

Also check calibration of equipment used during testing, was it giving the correct information?

 

Also important to know is the procedure followed during testing. For example in which steps was the test pressure applied, and was the temperature of the water / material during testing.

 

Met vriendelijke groeten / Best Regards,

 

Herman Pieper

QA-QC Inspector / CSWIP + IWI-C Welding Inspector / IWT / Materials Expert

 

Job van der Havestraat 6

8384 DB, Wilhelminaoord

Cell: +31 6 51691215

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]
Verzonden: maandag 22 februari 2016 08:55
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:24349] RE: 24334] Failure Analysis

 

If possible, you can also take a radiography in the same line of failure (seam or seamless) 

to check for any defects in that pipe material. 

 

C Sridhar.
Technical Adviser - Welding,
for Alsta Pristine Engineering Private Limited,. Bangalore
( SS, AL fabricators & A venture of Advance Eng. Training & Inspection Services). Chennai,

Mobile nos: 0 94449 71097, 0 7406 326326, .

 

 

Please don't print this e-mail unless you really need to. Save the environment.

 


Life is like bicycling. To move on, keep balancing  throughout.. 


 

 


From: 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>; Nachiket Vagal <nachi.vagal@gmail.com>
Sent: Monday, 22 February 2016 10:10 AM
Subject: Re: [MW:24345] RE: 24334] Failure Analysis

 

Thanks, Alan. I have asked for more details as it is of a great general interest to all students of failure analysis. I shall make them available on this forum when received.

 

BR,

Shashank C Vagal 

 

 


From: Alan Denney <alan@denney1.freeserve.co.uk>
To: materials-welding@googlegroups.com
Sent: Monday, 22 February 2016 3:08 AM
Subject: [MW:24341] RE: 24334] Failure Analysis

 

 

Alan Denney

AKD Materials Consulting Ltd

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]
Sent: 21 February 2016 08:51
To: Bathula Raghuram (Mumbai - PIPING) <r.bathula@ticb.com>; Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24334] Failure Analysis

 

Dear all,

Please suggest what could have caused this pipe failure after Hydrotesting..... Consider all general conditions as all details are not known yet

 

BR,

Shashank C Vagal 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/434548542.6153632.1456044675941.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

 

This email has been scanned by BullGuard antivirus protection.

For more info visit www.bullguard.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000801d16cf0%2435111d80%249f335880%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1737111366.6375486.1456116044537.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2051398195.6417657.1456127671999.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...