Re: [MW:24318] Re: Hardness Of P-91 Material

MINIMUM PWHT TEMP IS 730 DEG CELSIUS. ITT IS BETTER TO DO AT 760+- 10 WITH  30MINUTES MINIMUM

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Thu, Feb 18, 2016 at 2:13 PM, <afrozshaikh2007@gmail.com> wrote:
Dear Kumar,

Please do the PWHT By Induction heating method and keep the heating &cooling rate 80 -100 Deg C.Also do post heating for 4 hours.

Regards,
Afroz Shaikh

On Saturday, January 30, 2016 at 10:44:02 AM UTC+5:30, pradipsil wrote:
Dear Everybody,

Some of our P-91 Joints( Weldment) are coming hardness value around 300HB in the HRSG Unit.
 Joints thickness is 18 mm & 20 mm & we did PWHT 2 hours holding time at 710 degree centrigrade also we did 150 degree heating rate ,120 degree cooling rate.

Can you pls suggest us this hardness value  is acceptable in the HRSG unit. If not pls suggest me how to recover.
Regards,
Kumar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4958d285-a029-4b80-945d-1466c2fd8373%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eP%3DuznTTUK6G%3DXrgrj72XJF-jZ%3Dv%3D61uDUxDvc81uNYGA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...