[MW:24415] PWHT

Dear all,
I have two queries:
MOC: P8Gr1(SS347 internal)
PWHT on job with LAS is at 705+/-10 degree C for 10 hrs.
Available PQR: 700 degree C for 8 hrs.
Can I support same PQR for welding of SS347 internal which will undergo PWHT at 705+/- 10 degree C along with LAS???

Impact: not applicable for SS.

Second query:
Interpretation of QW407.1 (b).

Regards,
Maulik

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFK0MUMCrJL9dRmq0Q%3DDEJpfNmP%3DJ%3DRmrTk4fzV7cjfUj7FKdw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...