[MW:24349] Acceptance for bottom plate of storage tank (API 650)

Dear Experts,

We found 42 mm distortion in bottom plate after welding with shell. Is it acceptable? Please share reference standard. 
Please note tank fabrication is going on within shop.

Br,
Vishal Sharma

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAK1segupjbGRtScdgV3DhDP4k-7sx2y_NjnfcBC8fovg-g6ag%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...