Monday, February 22, 2016

[MW:24345] Re: Calculation for welding rod requirement for SMAW



Dear Tahir ,

Please find attached welding rod calculation for your refference and verified it with actual consumption at site.

Regards,
Afroz Shaikh
IOTL
On Monday, February 22, 2016 at 9:23:03 AM UTC+5:30, tahir alam wrote:
Dear experts

Kindly guide me how to calculate welding rod requirement for SMAW welding process for Plates,(storage tank construction)

1)Fillet weld
2)Butt welding-single V and double V



Best Regards
Tahir Alam
Planning Engineer
Agam Tank Maintenance Group
Mobile : +(965)5150-1509


--------------------------------------------------------------------------------
Site Office : +(965)2388-3614
Head Office : +(965) 2398-5381l2
Fax : +(965) 2398-8312
P.O.Box : 9390 Ahmadi, 61004 Kuwait
Email : tahira...@gmail.com
Website : www.agamltd.com
-------------------------------------------------------------

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eef782b9-e897-4d2d-882b-189252fe7b15%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...