Dear sir,
For welding of S690QL#S690QL, you should go for ER100S-G.

Regards,
Maulik

On Jan 28, 2016 4:46 PM, "BILLY TAN" <bil19875539@hotmail.com> wrote:

Hi Experts

I am currently developing WPS based on ISO 15614-1.
If I am using ER 70S-6(lower strength wire)(GMAW process) to weld weldox700 /SQL 690 to weldox700 /SQL 690, will I face any problem to weld on it except on the tensile strength? As the tensile strength needed for the structurer is just like S355 material. It is understood that it violate the code ISO15614 on tensile strength. The weldox material is selected base on the wear and tear purpose.


Best Regards
Billy

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/COL131-W73B5F382CCDE066A11CDF3A5DA0%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFK0MUMeDz6ngZSi9x3Lr%2B2Y4rjXHXU99cbCdWpJ9ONcvnzxmw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...