Dear All,
What is the thumb rule to consider consumption ratio if different sizes of electrodes (2.5,3.15 & 4mm) for structural works of different thickness
I am considering 2.5 mm with 25% consumption, 3.15 mm with 50 % consumption & 4 mm with 25% consumption , is it ok?
Regards,
Afroz Shaikh