Thursday, January 21, 2016

Re: [MW:24144] Fwd: mode of metal transfer

Dear sir,

With usage of E71T-1C filler wire one can achieve spray like metal transfer (droplets are larger then normal spray droplets) with CO2 due to flux formulations.

One can not achieve true spray transfer in case of FCAW.

Regards,
Maulik H. Thakkar
Welding Engg & Metallurgy
Larsen & Toubro Limited.
India.

On Jan 18, 2016 5:41 PM, "udaya bhaskar" <dusroni@gmail.com> wrote:

Dear experts,

Please clarify which mode of metal transfer we are used  in FCAW 

 Welding Process : FCAW
Gas                      : co2
Filler wire             : AWS A5.20 71T-1C
Mode of metal transfer : ? (Please clarify )


--
With Regards

Udyabahaskar.D

+919676270121

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RN2REbTDX4rvKdo1oUtWMZMz09KaPEPi9TLi70tg5M-BQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFK0MUPMXW98xP9AYoPWnTz0oRaWtsgGGfYse96c4DxjY88D8w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...