Its available in market, Niton series machine is having that capacity…Just go to the web site or supplier, will provide all relevant information

 

Thanks & Regards,

Mohd. Azam

Doha- Qatar


On Fri, Jan 22, 2016 at 10:00 AM, chinmayee4 . <sivayya.a@gmail.com> wrote:
Yes, There is a machine called   XMATE 2000.  you will find internet.  There are some XRF models . 

On Sun, Jan 17, 2016 at 10:14 AM, 'Biplab Pal' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Friends,

Can you please guide me if there is any portable PMI machine(fit for use any condition) available  which can measure Carbon content.
I will appreciate if you send me the Catalog (If any).

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg0C2Mf68MEi9H8KuxU9K6EF%2BcvZskpeCSa19UYUrfop8w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks with Regards


Sivayya
Competent Person 
D. NO. 13-32/15, F. No. 107, 
SVLN Paradise -1, NAD Layout, 
Chinamushidivada,
Opp. Sujatha Nagar. 
Visakhapatnam - 530051
Mobile : 9346868777

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFx%3D0kGVM%2BZ87F%2BAZzz%3DD7B4eM_UEerPkuQ2M5BnR2GVb308pA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXS%3D1Kuk6zV2drWrBsn0Y%2B032W-c1ua8OyzS_DwM28QRmA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...