Re: [MW:24130] Qualified thickness for welder

Hi Mr Anamul,

For qualification mentioned in below mail ,thickness qualified is unlimited. Refer para QW-452.1b.
Note that Para QW-404.30 cross refers para QW-452.1b for performance qualification by radiography.
For position qualification refer para QW-461.9.
The welder is qualified to weld flat position for size less than or equal to 24" pipes and flat & vertical position in size more than 24" pipes.

hope this clarifies you.

Best regards,

Padmasanker.s
Project quality coordinator,
Bilfal heavy industries ltd.

On 19 Jan 2016 05:25, <anamulqc@gmail.com> wrote:
Dear Sir,

 We conducted welder qualification at Karbala Oil Refinery Project as per ASME-IX 2013 Edition. 

 WPS details as follow 
1. WPS qualified base metal- P1 to P1 Gruop all
2. WPS mentioned base metal thickness range- 5 to 26 mm
3. Process FCAW
WQT details
1. Joint design Single V butt joint with back weld(Root side back grind then weld)
2. Base metal SA283-C
3. Thickness 16.0 mm
4. Sequence of welding- Root pass>Hot Pass>Filling>Capping>Back grind & Back weld
5. Test position 2G & 3G 

My client inspector say welder will qualified only for 2T  & Pipe Diameter will qualify over 24" I want to clarify is he correct? For thickness qualified he mention about QW-404.30 
However I will appreciate to you for clarify my problem.




Regards
Anamul
QA/QC Engineer


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b86d11c7-1ff9-4ee6-b63e-040e6aafcdbe%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKDH8GpKrPp-uZ_7ObMt2g6UxW7CcmFMReOwR1C1n0xaNagSMQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...