Sunday, January 31, 2016

[MW:24193] Hardness Of P-91 Material

Please ref ASME B 31.1 TABLE NO. 331.1.1 or NACE MR 0103 for hardness requirements and also maintain voltage & amps less than required ileveln each layer to obtain hardress valve with in limit