Yeah . I my idea , cause the spec aws d1.1 did not show how to qualify a welding repair procedure , so I think we can use the wps that we are already running on for build new structure to use for repair procedure .
In detail: if u have wps SMAW process for fabricate new structure, u can use that wps for repair also .
Kindly share my idea , if all experts here have any confirm or right info , please show with us
Thanks all experts
Tuan QC inspector
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4b0f0e69-fc20-43ba-9ed0-47ea432e75c3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
In detail: if u have wps SMAW process for fabricate new structure, u can use that wps for repair also .
Kindly share my idea , if all experts here have any confirm or right info , please show with us
Thanks all experts
Tuan QC inspector
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4b0f0e69-fc20-43ba-9ed0-47ea432e75c3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments