Re: [MW:24119] Ferrite No. in Austenistic stainless steel weld overlay in FCAW process

High dilution rate might be a reason

Sent from my BlackBerry 10 smartphone.
From: Bhatt Purvin
Sent: Σάββατο, 16 Ιανουαρίου 2016 - 17:44
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:24106] Ferrite No. in Austenistic stainless steel weld overlay in FCAW process

Hello,

I find it bit strange to receive Ferrite no. above 8 or up  to 11 some times, while using FCAW weld overlay on CS surface. What are the reasons behind these. 
My requirement is 3 to 8 % only. 
Can  I have any solution for this ? .
 PWHT  will be there in my job. 
What should I do to restrict up to 8 % only, with same process.  

Warm Regards
Purvin Bhatt 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/075922ad-610d-4296-b6a6-b04d12b687e0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...