If your fabrication is governed by ASME Boiler and Pressure Vessel Code the answer is unequivocally NO. You need to perform a qualification with P5B and P8 materials.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of JIJILAL K M
Sent: Wednesday, January 27, 2016 2:38 AM
To: materials-welding@googlegroups.com
Subject: [MW:24176] can use P15E wps for P5B
Dear Experts,
We've to weld 4" x 6.02 mm HRSG boiler piping joints (only 2 nos.).
Materials are P5B + P8 ( ASTM A335 P5 + ASTM 304L SS) .
There is no such qualified WPS.
instead we've a Qualified WPS for P15E + P8 ( ASTM A335 P91+ ASTM 358 316L SS) .
Can we use this WPS using filler wire ER-309?
JIJILAL K.M.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHjed5vcPCO0Xcu9BL0jh%2BF8oD6fc2qgxXLpHejBsZU5dA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments