That depends on many things including the alloy used to make the bolt. The bolt would not be used at stresses where it sees more than very low levels of elongation. Why do you need this information?
Alan Denney
AKD Materials Consulting Ltd
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthikeyan Shanmugananthan
Sent: 23 January 2016 06:38
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24163] Material properties
Dear Experts
How to find out maximum limit of elongation % for B7 Grade bolts (SA-193). All the standards are specified minimum elongation % only. Kindly refer some tips to proceed.
Regards
S.Karthikeyan
Chennai
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/44cf1ab8-06dc-4141-8bf4-d4c64beae1fe%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/001101d155b5%245dc66660%2419533320%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:35754] interpration
Interpretation #: BPV IX-18-34 Record Number: 18-771 Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment