Friday, January 15, 2016

[MW:24094] Define welding engineer

My company need to qualify wps follow aws d1.1 :2010 . And we do run pqr by testing internal, witness test piece . Only send test piece to third party LAB to bend test and RT. But not have third party witness all process from starting. So my question is : do we do wps right with spec aws d1.1
- does spec or code require wps must have third party to witness , cause I can not find any information about it

Thanks very much all experts
Tuan QC inspector

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1b8824bd-f8f8-4272-9ce1-de21585a0051%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...