Re: [MW:24128] what is the difference between QAP and ITP

ITP is given by customer which covers only main inspection calls e.g. full component after welding UT of only some joints, final machining dimensions and after assembly inpection whereas QAP is made by the manufacturer which covers all the stage wise inspection..

On Tue, Jan 12, 2016 at 4:14 PM, Pradip Ghosh <pradipg2@gmail.com> wrote:

Can any one provide me a details explanation of difference between QAP and ITP.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d5107353-54a0-49a9-9d23-6123ee54d599%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKaLp%2BVeSfvN1fLsv_-qmu0uPZk4C_HpwW305agu3y9TgPM-YA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon