Dear all,

1st thanks for your kind support.

So we are in conclusion of 2 as all people suggested.
As per ASME B 31.3 if we are qualifying a WPS the following shall apply.

Case 1. If thickness of test piece is less than 6mm then qualification range will be 1/2t to t+6.
    If thickness of test piece is above 6mm then qualification range will be either 16 or t to t+6.

Case 2. for all 1/2t to t+6.


Please provide your input which one is correct case 1 or case 2 ??


Thanks & Regards


On Sat, Jan 16, 2016 at 1:01 PM, Vino Varghese <vinopvarghese@gmail.com> wrote:

One has to refer the applicable Construction Code for the Impact test requirement. If its, ASME B31.3, you need to follow the same.

Regards, Vino

On Jan 16, 2016 7:22 AM, "Raghuram Bathula" <raghurambathula@gmail.com> wrote:
yes construction code (B31.3) limits will apply

On 13 January 2016 at 14:01, 'Biplab Pal' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Experts,

If impact test is required for any WPS the base metal thickness limit is an supplemental material and qualification of minimum thickness limit shall follow QW-403.6.
Now our Consulting Service Department is telling us the qualification thickness limit shall be t/2 to t+6mm. as per ASME B 31.3 table 323.3.1 for piping.

Guys, did you faced this kind of problem? I am experiencing this problem 1st time.
Please let me know your understanding and experience.

--
Thanks & Regards
Biplab Pal
Welding Inspector

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3D4cuWpumsK2-NACzY%2BM4Sun-tXbVgVCDXRcDnkta%2Bt_Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7BZGzcYBq8p66Ei1oB7ZO50fZ52g%2BAPDrJyoam0REp3Cg%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.



--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg2SPaHbsgeNqROKnmMKMST78qg_2d0Tm_ovE7%2BX%2BxUCBg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...