[MW:24193] Size deviation - Female Sprinkler adaptors

Experts,

 

 

We have received  Female Sprinkler Head Adaptor 3/4"* 1/2" size.This adaptor shall be made socket weld with 1" Pipe. But ID for the 1" pipe is 25 mm and id for Female Sprinkler Head Adaptor 3/4"* 1/2" is 27.5 mm (Pls see the attached pics ).

 

If we weld Pipe to adaptor , we will not be able to get Weld penetration with this size deviation.


Can we do Butt Weld in this case?

 

Kindly advice.

 




Best Regards,

 

Krishana Kamal Nayan

QA/QC  Engineer

Weatherford Oil Tool Middle East Ltd. |

Mobile:+964 780 925 0270

Krishana.Nayan@ME.Weatherford.com  │ www.weatherford.com

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN%2Bgo9APsBDa3J1V1hzVONFetLkyZq9Sa_zoEKgUAVDO1Ee%3DNg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...