Re: [MW:24106] PQR position conflicts

DEAR PRAKASH SIR,
                                 QW203 SAYS WPS QUALIFY IN ANY POSITION QUALIFIES PROCEDURE FOR ALL POSITION AND QW405.2 SAYS CHANGE FROM ANY POSITION TO VERTICAL UP. VERTICAL UPHILL PROGRESSION QUALIFIES ALL POSITION. MEANS IF MY WPS IS QUALIFY FOR 1G THEN IT QUALIFIES ALL POSITION OR NOT? AND IF THERE IS PWHT OR IMPACT REQUIREMENT THEN WHAT'S THE LIMIT? PLEASE HELP ME TO UNDERSTAND.

On Monday, January 11, 2016 at 9:28:30 AM UTC+5:30, Prakash Hegde wrote:
Hi!
As per ASME code
I) If PQR is qualified in 3G having Impact test requirement  for equipment  in such case you can qualify welder for any position based on this relevant PQR and WPS as per requirement
(For Impact test requirement  Welding position is essential for PQRi.e. 3G)
ii) If PQR is qualified for Non Impact test requirement(Even in 1G position ) in such case you require to qualify welder in any position as per requirement
Regards
Hegde P.B.



On Saturday, 9 January 2016 4:31 PM, Peter Soloman <peterv...@gmail.com> wrote:


Dear,

PQR is qualified but welder is not qualified for 6G position.

regards
peter soloman

On Mon, Dec 7, 2015 at 4:00 PM, Narender Reddy <malgire...@gmail.com> wrote:
Dear experts

As per sec IX

I have an PQR which qualified on 3G(Plate) so


Q.1) Can i use that pqr for to weld 3Nps pipe 6g positions welding.

or is there any conflict between plate and pipe qualification.If there experts can explain why?

Bets regards
reddy.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eefd149c-2943-4be7-901c-68dc59be172c%40googlegroups.com?utm_medium=email&utm_source=footer.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMvP5syom%3DgwBQ800tM9RvOaBR9zjrVtLwqohrnd7K9gZxn_CA%40mail.gmail.com?utm_medium=email&utm_source=footer.
For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4cb0b2cc-8f74-4f91-8c99-c8b44bdab354%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...